Hi

I've had a problem with a couple of infused parts not releasing from the molds this last week, the problem appears to be my easylease has gone 'off', i've had it about 14 months.  Anyway two of my molds are a complete mess and there is definitely no way they are useable or repairable, the third, pictures below has, has this crazing pattern in quite a few areas and some cracking in places on the edge.  Would I be correct in thinking that this is scrap too?

http://i1049.photobucket.com/albums/s386/Andrewt1971/IMAG0038_zps728a9b1b.jpg

http://i1049.photobucket.com/albums/s386/Andrewt1971/IMAG0041_zpsf41bce34.jpg


thanks

andy
Edited 12 Years Ago by andrewt1971