Can anyone tell me the best way to cut aluminium core? We use water jet to cut core and CNC machine to mill it. But i was looking for a manual method. I have tried desouter (diamond) cutter but it simply melts down the metal. I have also tried bandsaw cutter which gives a good finish but very difficult to control the tolerances.

Any Brighter Ideas??