StanTheMan
StanTheMan
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 61,
Visits: 380
As the title suggests, anyone got any sources for the 4x4 twill fabric? Just dry fabric, no prepregs. Thanks in advance fellas
Regards,
Stan
Reply
Like
3
Tominator
Tominator
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 9,
Visits: 320
Try these guys. Pretty decent prices too.
http://www.solarcomposites.com/composites/compositecarbon.html#6K
Reply
Like
6
StanTheMan
StanTheMan
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 61,
Visits: 380
Yeah, I know them but they're in the US. I'm trying to avoid paying VAT for importing outside the EU and cut the delivery times by quite a margin hence the "EU" in the title
Reply
Like
3
compositepro
compositepro
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 22,
Visits: 65
http://www.cristex.co.uk/products/woven-fabrics/6k-carbon-balanced-fabrics
Reply
Like
3
r0bsk1
r0bsk1
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 38,
Visits: 307
Try here....
http://www.fibermaxcomposites.com/shop/-p-295.html
Very quick to deliver too.
Reply
Like
3
StanTheMan
StanTheMan
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 61,
Visits: 380
Awesome guys! Thanks!
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search