Oil Mist Eliminator for vac pump
Oil Mist Eliminator for vac pump
Post Reply
Like
10
Oil Mist Eliminator for vac pump
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
carboncactus
carboncactus
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 243,
Visits: 1K
That looks like it's gonna break within 2 days, lol.
Reply
Like
10
Heresy Miniatures
Heresy Miniatures
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 1,
Visits: 8
Hi
I'd like to get an Oil Mist Eliminator for my Easy Composites 12cfm vac pump
This:
Oil Mist Eliminator (available in USA)
seems to be the sort of thing, although I've also seen two-stage exhaust filters that can also return the oil to the pump, which seems like a good idea.
Would any of these:
(UK site for exhaust filters)
fit the pump or can you recommend something that would? Not really practical to vent the exhaust fumes from the room - no windows, or outside wall, etc.
Any advice appreciated
ta
Andy
Tags
exhaust fumes
oil
vacuum pump
Reply
Like
10
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
10
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search