You can certainly bring the mould to show us and discuss layup etc. We specifically allow time in the course to discuss personal projects.
However we generally do not allow customers to mould from thier own moulds due to the way we run the course. We normally have 2 people working on each mould that we set up, so if one was getting a part for himself out of it and another was not, people may consider it unfair. Also the moulds we supply have been chosen to have certain features that test your skills which your mould may not have in the same way.
Thus we supply moulds and if you are staying longer on the other courses you can demould the generic parts youve made. If, however, you were coming as a group of workmates and wanted to bring the mould that way, we may consider it dependant on mould size, shape etc.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|