posted 14 Years Ago
ANSWER
HOT
Topic Details
Group: Awaiting Activation
Posts: 4,
Visits: 44
Hi guys, I just tried to do a resin infusion (doing it as a hobby, glassing wings for model aircraft) in the garage and the resin just didn't want to play ball. After 5 hours of using a heat gun to get the resin to flow into all the spaces on the wing (doubly hard to do the top and bottom of the wing at the same time) and the damn stuff just wouldn't shift, what's the minimum working temperature for this stuff. It's been a cold night, started at 4 deg and it went down to -1 deg. I know the pot life is 40-60 mins, I guess I stuck with it out of desperation as the wing alone took 38 hours to shape
. Any input would be great, thanks guys.
CJ
Reply
Like
8
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Infusion resin properties
CJ
-
14 Years Ago
Hi and welcome CJ. Temperature: It is vital that the temperature of the working environment is...
Paul (Staff)
-
14 Years Ago
Hia, thanks for the reply, I fear it's too late to recover the peice, a second inspection with fresh...
CJ
-
14 Years Ago
Oh nooo... I had the same issue 3 days ago! wish this post was already up! fortunatly i wasn't doing...
MAVERICK
-
14 Years Ago
If you going to out it in a box I would make a hole in the back the size of the outlet of the...
CJ
-
14 Years Ago
I Agree with CJ on the getting some ventilation in the box, should make it a fair bit safer, your...
Aero Steve
-
14 Years Ago
Thanks for the tips on the release film and peel ply, I don't pull a full vacuum when I do my foam...
CJ
-
14 Years Ago
Hi CJ, No I'm not on RC groups, good tip on dropping the vac a little, I'll give that a go on the...
Aero Steve
-
14 Years Ago
Post Reply
Like
8
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search