Unfortunately we don't have that data for the resin, and the manufacturer hasnt got it to give us either.
The reason you unlikely find that data is that the resins are not used on thier own. They are part of a composite thus the data given is only really representative and of little use other than comparing between resin systems.
The figures would be massively different in a composite laminate.