Hello everybody.

I would thank you any ideas about how to manufacture the chair which is in the attached file. I think the best method would be vacuum bagging. And later, I can refinish the rear side with extra layers of epoxy resin plus sanding & polishing until nice shine.

My problem are the "legs" and the back of the chair. Tha legs have a triangular section, so i could use a core made from PUR foam? or maybe othe best options?

But the back in crushing my head. These designers dream a lot....
Thank you for your comments.
                                                
Attachments
carbon fiber chair.pdf (592 views, 1,007.00 KB)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search