Group: Forum Members
Posts: 26,
Visits: 264
|
Yep, you read that right.
If you want the door trims done that's 600 but for all interior trims is 1000. That's if you send them your trims to be skinned, or alternatively pay an extra 400 then they skin some for you, send them to you then you get a refund of 350 when you return your factory parts back to them.
So, rather than pay the GBP equivalent of USD1000+ I am having a go at the process myself.
Originally I was mixing epoxy basecoat and hardener 1:1 then realised it's meant to be 1:0.5 so that fixed one of my first issues. Now I realise I have laminating resin instead of coating resin so I've ordered some coating resin from easycomposites and I am hoping my attempts will be alot better from now on.
|