carboncactus (15/06/2013)


I like robs super glue method. How do you keep it tidy? Stuck fingers guaranteed if I do it!


Erm...carefully!Smile Dont use too much and keep a spoon handy just incase.
Jess8bit
Jess8bit
Supreme Being (843 reputation)Supreme Being (843 reputation)Supreme Being (843 reputation)Supreme Being (843 reputation)Supreme Being (843 reputation)Supreme Being (843 reputation)Supreme Being (843 reputation)Supreme Being (843 reputation)Supreme Being (843 reputation)
Group: Forum Members
Posts: 133, Visits: 566
carboncactus (15/06/2013)
Oh you mean the edge as in the thickness of the part? To seal it from humidity? 
yep !
I tend to clear coat my parts so the overspray takes care of it, but you're gelcoating then trimming.
ok, usually I don't clear coat them.

I like robs super glue method. How do you keep it tidy? Stuck fingers guaranteed if I do it!
LOL
carboncactus
carboncactus
Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)
Group: Forum Members
Posts: 243, Visits: 1K
Oh you mean the edge as in the thickness of the part? To seal it from humidity? 
I tend to clear coat my parts so the overspray takes care of it, but you're gelcoating then trimming.

I like robs super glue method. How do you keep it tidy? Stuck fingers guaranteed if I do it!

http://www.talkcomposites.com/Uploads/Images/db628ad5-e0e7-47b9-873a-3d84.png
Jess8bit
Jess8bit
Supreme Being (843 reputation)Supreme Being (843 reputation)Supreme Being (843 reputation)Supreme Being (843 reputation)Supreme Being (843 reputation)Supreme Being (843 reputation)Supreme Being (843 reputation)Supreme Being (843 reputation)Supreme Being (843 reputation)
Group: Forum Members
Posts: 133, Visits: 566
@cc : Black satin is really nice. I luv it. But it changes the whole color of the part, which is not what the customer necessary desires Smile But I'm astonished how it has hidden the bridge on the lip 
I need to find some black stain coat !

@r0bsk1 : ok for cyanoacrylate glue Smile
r0bsk1
r0bsk1
Supreme Being (340 reputation)Supreme Being (340 reputation)Supreme Being (340 reputation)Supreme Being (340 reputation)Supreme Being (340 reputation)Supreme Being (340 reputation)Supreme Being (340 reputation)Supreme Being (340 reputation)Supreme Being (340 reputation)
Group: Forum Members
Posts: 38, Visits: 307
Seal the edge with Cyanoacrylate, lightly sand until smooth then polish.

Or if you have a core to cover up use black gel coat.
carboncactus
carboncactus
Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)
Group: Forum Members
Posts: 243, Visits: 1K
Do you wanna hide that bridge you had earlier?

I had a pretty bad bridge with a nosecone. You an sort of see it, it's in the lip at the back:



I covered it with some black satin using 3M fine line tape:



http://www.talkcomposites.com/Uploads/Images/db628ad5-e0e7-47b9-873a-3d84.png
Edited 12 Years Ago by carboncactus
Jess8bit
Jess8bit
Supreme Being (843 reputation)Supreme Being (843 reputation)Supreme Being (843 reputation)Supreme Being (843 reputation)Supreme Being (843 reputation)Supreme Being (843 reputation)Supreme Being (843 reputation)Supreme Being (843 reputation)Supreme Being (843 reputation)
Group: Forum Members
Posts: 133, Visits: 566
After trimming/sanding, how do you finish the border ? I've heard some people use a small brush with black gel coat ?

Smile
Jess
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search