Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Resin Infusion
»
How do I create a vacuum seal around silicone hosing?
How do I create a vacuum seal around silicone hosing?
Post Reply
Like
5
How do I create a vacuum seal around silicone hosing?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Chris B
Chris B
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 5,
Visits: 25
Hey guys. I'm doing research on composite materials in the US, and I've scoured the internet looking for an answer to this question, so I'm asking you guys for help.
First, pictures of my set up:
http://i.imgur.com/VAfDkGV.jpg
http://i.imgur.com/zqhy5a2.jpg
The hose leading to the right goes to my resin jar, and the one on the left goes to my catch jar.
Some background: the resin/hardener system I'm using is EPON 862/Agent W. I've never worked with it before, and it has 5 cure cycles at 2 different temperatures: 250 F and 350 F (121 C and 177 C). This led to issues with the PVC tubing as it melted when I placed it in the furnace. I noted it and got silicone rubber tubing from another supplier as it can withstand the higher temperatures.
My issue arises when I attempt to create a vacuum seal in the bag. The sealant tape doesn't stick to the silicone tubing and thus can't hold a vacuum. I'm searching for a solution to this problem. I noticed Easycomposites sells silicone tubing for high temperature use, so I figured this community might have a solution to the problem.
Things I've tried so far:
My most successful solution was to take a small piece of brass tubing and put the sealant tape on that, then attach the silicone tubing to the brass tubing. It (strangely) holds a decent vacuum, but tiny amounts of air still leaks in.
I've tried using sandpaper to rough it up a bit. Doesn't work.
I've rubbed acetone on the outside of the tube. Doesn't work.
I've tried black sealant tape, which is slightly tackier than the yellow stuff. It doesn't really work either, plus the black tape doesn't go up to the temperature I need it to.
I've tried wrapping paper around the tube before placing it on the gum tape. Shouldn't be surprising that doesn't work.
Any tips?
Tags
hosing
silicone
tubing
vacuum
Edited
13 Years Ago by
Chris B
Reply
Like
5
Replies
Chris B
Chris B
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 5,
Visits: 25
carboncactus (13/06/2013)
The problem is the resin which cures at a high temperature. Standard resin infusion is out the window since you can't use pvc tubing and vacuum connectors. At those temperatures, you have to use a silicone hose.
Interesting. I never realized how much of a pain working at 350 F is (I mean, I can bake a cake at that temperature).
The barbed fittings are a good idea. I may try that. I could probably get some mold release agent inside of it so that I can reuse them (assuming that the metal can withstand the chemical reaction).
Reply
Like
6
Matthieu Libeert
Matthieu Libeert
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 955,
Visits: 3.4K
you could also just drill them out, if resin hardened in the metal part
Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com
Reply
Like
7
Chris B
Chris B
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 5,
Visits: 25
matthieutje65 (13/06/2013)
you could also just drill them out, if resin hardened in the metal part
Genius. I never thought of that. Thank you.
Reply
Like
5
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
How do I create a vacuum seal around silicone hosing?
Chris B
-
13 Years Ago
I think the answer is simple... use a vacuumbag-connector and all your problems should be solved :p
matthieutje65
-
13 Years Ago
I could do that, but I would still need to run the hose through the vacuum seal in order to get the...
Chris B
-
13 Years Ago
Silicone releases naturally, so you'll have trouble sticking anything to it, even though it makes a...
carboncactus
-
13 Years Ago
Thats how I do it for vacuum infusion skip to 5:54 min...
matthieutje65
-
13 Years Ago
carboncactus: I thought of using a zip tie to wrap around the tubing and then adhering that to the...
Chris B
-
13 Years Ago
The problem is the resin which cures at a high temperature. Standard resin infusion is out the...
carboncactus
-
13 Years Ago
[quote][b]carboncactus (13/06/2013)[/b][hr] The problem is the resin which cures at a high...
Chris B
-
13 Years Ago
you could also just drill them out, if resin hardened in the metal part ;)
matthieutje65
-
13 Years Ago
[quote][b]matthieutje65 (13/06/2013)[/b][hr]you could also just drill them out, if resin hardened in...
Chris B
-
13 Years Ago
Hi Matthieu :) Watching your helmet tutorial, I've noticed you use a special composite glue spray....
Jess8bit
-
13 Years Ago
Post Reply
Like
5
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search