Easylease claims to be a sealer/release agent all-in-one. I don't know how, as every release I've used requires 2 applications of their respective sealers (Chemlease, marbocote etc). However, I think pinholes are rather large for any sealer to cover. They normally seal microscopic porosity, and they wont even cover 1200 grit scratches.

You are gonna have to fill the pinholes somehow. This depends on what your mould surface is made of though.

http://www.talkcomposites.com/Uploads/Images/db628ad5-e0e7-47b9-873a-3d84.png
_GABBER
_GABBER
Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)
Group: Forum Members
Posts: 41, Visits: 646
G50 is a gel coat, ok, if you use it you don't have pinholes into the part. But i'm talking about the mold surface. If you have a little bubbles of air in the gel coat, or dust when you apply PVA, the mold surface has pinholes. Easylease isn't a sealant, so it doesn't fill these pores, and the surface of your part will not be smooth, besides having a more difficult release of the part
Daz
Daz
Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)
Group: Forum Members
Posts: 93, Visits: 651
I USE easylease then g50

Once out of mold flat the pinholes off
_GABBER
_GABBER
Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)Supreme Being (269 reputation)
Group: Forum Members
Posts: 41, Visits: 646
There is a sealant for pinholes, to apply before easy-lease? This release works very well, but it the mold has pinholes, it would be necessary a sealant