How about if I used carbon/kevlar for the 1st layer and carbon for the second layer and another carbon/kevlar for the final layer. Will that be sufficient? do I really need soric?
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
For a non caged car (and even for a caged car really), I would recommend at least one layer of kevlar or carbon/kevlar somewhere in the layup.  main reason being to keep the roof in one piece (albeit cracked and bashed in) in a roll over based crash, and also to prevent lots of carbon splinters coming into the cabin.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Daz
Daz
Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)
Group: Forum Members
Posts: 93, Visits: 651
I USED 2 OUTER LAYERS OF CARBON 1 SORIC AND ANOTHER CARBON

VERY STRONG .
vlcz85
vlcz85
Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)Junior Member (14 reputation)
Group: Awaiting Activation
Posts: 2, Visits: 15
Hi, I want to make a carbon fibre or carbon kevlar roof for my car. Just want to know which material suits better and how many layers should I use in the resin infusion.