How and Why to Vacuum Degas RTV Silicone Rubber and Casting Resins


How and Why to Vacuum Degas RTV Silicone Rubber and Casting Resins
Author
Message
Warren (Staff)
Warren (Staff)
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Welcome to another of our video tutorials.

The purpose of this Video tutorial is to demonstrate the benefits of degassing materials like RTV silicone rubber and casting resins (like Fast Cast polyurethane or water-clears) to improve your moulds and castings.

We use our Complete Vacuum Degassing System and demonstrate how simple the process is and why we do it at various stages such as during silicone mould making, before pouring casting resins and also in-mould degassing.



For a complete list of all the products used in the video, please view the project (in full HD quality) in our Online Composites Learning Centre.

We hope you like the video!

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Edited 13 Years Ago by Warren (Staff)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search