Group: Forum Members
Posts: 33,
Visits: 187
|
I applied some coating resin to a part about 2 weeks ago. and even now it is still slighlty tacky to the touch. Weirdly the excess resin in the mixing pot seems to have cured fully and is not tacky. I used a digital scale and am pritty sure I mixed it 2:1. The part is made from glass cloth and EL1 laminating resin. Any idea what could be the cause of the tackyness, and any way I could salvage the part? It took me quite some time to make the part so I'd really hate to have to toss it.
|