prsw (13/05/2013)
Is that UD I see on the side?
Did it infuse good?
I did a self-supporting racebike subframe with lots of UD and didn't infuse because it, I have been told, does not wet out if infused.
(or rather i did infuse it first and then wetlay/bagged more material later.)

Bartonphoenix750 (28/04/2013)




Hi

No it is 200g twill.

Regards Chris

http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search