prsw (13/05/2013)
Is that UD I see on the side?
Did it infuse good?
I did a self-supporting racebike subframe with lots of UD and didn't infuse because it, I have been told, does not wet out if infused.
(or rather i did infuse it first and then wetlay/bagged more material later.)
Bartonphoenix750 (28/04/2013)

Hi
No it is 200g twill.
Regards Chris