Clearcoat Fisheye


Author
Message
vnelen
vnelen
Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)
Group: Forum Members
Posts: 10, Visits: 68
Well I resanded my part with 1500.  Got a nice smooth matte finish.  And started the clearcoat.

Immediately I started seeing fisheye.  Of course more layers didn't help, it just got worse.

I'm going to resand it down.  But what can I do to fix this?
FLD
FLD
Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)Supreme Being (3.7K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
Sounds like you have pin-holes in the laminate.  These are microscopic holes in the weave of the fabric that the clearcoat wont fill if sprayed.  Flat it back as you have done previously.  Dilute some clearcoat twice what you would do for spraying.  Brush this on and work it into the surface with the brush as much as you can.  Let it go off fully then repeat.  Now spray it, should be fine then.
vnelen
vnelen
Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)Forum Guru (58 reputation)
Group: Forum Members
Posts: 10, Visits: 68
I took it back and there are a few thin spots now.  So I'm going to add another couple layers of resin and resand. Maybe that'll put me in a better place.