direction of the fiber
direction of the fiber
Post Reply
Like
3
direction of the fiber
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
+cosworth
+cosworth
posted 14 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 19,
Visits: 142
Importance of the direction of the fiber? Which is the way of doing?
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
direction of the fiber
+cosworth
-
14 Years Ago
Hi, Well, it depends on what you want to achieve, and which fabric you have. Is it unidirectional...
Joe
-
14 Years Ago
hello is for making a surfboard fin I am using 163g Light Weight Woven...
+cosworth
-
14 Years Ago
When I've seen fins they tend to have the fibres running at +/- 45 degrees (if your looking at the...
MAVERICK
-
14 Years Ago
depends on the area of the fin I am using the 4-layer thin area in the 12...
+cosworth
-
14 Years Ago
Sounds a bit heavy! Have you thought about shaping some foam as a core to make up the thickness...
Mr-Rob
-
14 Years Ago
hello fins are very thin 3 or 4mm thick
+cosworth
-
14 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search