New member + new to composites Harry Harrison (Field Cycles)


Author
Message
Harry Harrison
Harry Harrison
Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)
Group: Forum Members
Posts: 5, Visits: 33
Hello Talk Composites,

I am a small scale bespoke frame builder, building frames from steel in Sheffield UK. I build using traditional methods, fillet brazing, silver brazed lugs etc etc. I use these traditional methods but always look for opportunities to build in technical and functional improvements in to the frames. Have a look at my web site for more of a picture www.fieldcycles.com 

I am building a few frames with an integrated seat post like the images attached. I would like to replace the extended seat tube / seat post with a composite tube. My idea is to build a frame with a lug at the bottom bracket and the seat tube top tube junction and then bond in a carbon tube. Any advice would be greatly appreciated, things like clearances, bonding composites to steel would be really helpful. 

Ideally I would like to use a composite tube that has an o.d of 28.6 mm (1 1/8") so it will work with the seat post top I make.  

Thanks 

Harry 
Attachments
DSC_3769.jpg (626 views, 175.00 KB)
JohnB2.jpg (609 views, 358.00 KB)
JohnB3.jpg (597 views, 381.00 KB)
Replies
Kevin-Lee
Kevin-Lee
Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)Supreme Being (374 reputation)
Group: Forum Members
Posts: 44, Visits: 2.4K
Hi Harry,

Those bikes are amazing!

And I think the man who does the paintwork on those bikes knows his s*** too...

Kev.
Harry Harrison
Harry Harrison
Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)Forum Member (43 reputation)
Group: Forum Members
Posts: 5, Visits: 33
Cheers Kev,

I make the frames and my pal paints them, he has the right amount of O.C.D to do a fantastic job !! he paints the odd carbon frame so might be able to fit some carbon stuff in in the future.

Ta

H
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Harry Harrison - 12 Years Ago
wozza - 12 Years Ago
matthieutje65 - 12 Years Ago
Harry Harrison - 12 Years Ago
Harry Harrison - 12 Years Ago
Kevin-Lee - 12 Years Ago
Harry Harrison - 12 Years Ago
wozza - 12 Years Ago
Harry Harrison - 12 Years Ago
wozza - 12 Years Ago
neilb - 12 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search