Much below 15C and the epoxy will take days to cure if at all.  Lower temperatures really do slow up the curing process significantly.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
alimeikle
alimeikle
Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)Junior Member (5 reputation)
Group: Forum Members
Posts: 1, Visits: 4
Hi there,

I would like to epoxy a wooden hull with coating epoxy, but it says to work at 20 degrees Celcius.

The boat is outside on a Scottish island, so 20 degrees is not going to happen very often, and certainly not before June/July.

Is it possible to apply a coat at lower temperatures??

Many thanks

Al
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search