Group: Forum Members
Posts: 6,
Visits: 16
|
I didn't use a roller but I probably will next time. I used normal EL2 epoxy laminating resin and ended up using more than I thought I would making it quite expensive. I just realised, should I be using that uni-mould tooling resin? It seems so much cheaper, does this work with the clear epoxy gel coat or do I have to get the uni mould one?
|