Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Resin Infusion
»
Intensifiers caul plates
Intensifiers caul plates
Post Reply
Like
7
Prev
1
2
Jump To Page
Intensifiers caul plates
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
fgayford
fgayford
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 433,
Visits: 1.2K
I will second that. Please post some pictures.
Thanks
Fred
Reply
Like
3
chamindaj
c
chamindaj
posted 9 Years Ago
ANSWER
HOT
Post Details
c
Group: Forum Members
Posts: 1,
Visits: 2
Hello,
We are trying to use flexible heater blanket inside the caul (intensifier) plate to improve the resin flow around the contour edges. Current difficulty is making the smooth heater surface that can use to attached to the caul plate. Any body have think of this idea. if so please advise.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
7
Prev
1
2
Jump To Page
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search