hi, i have wet laid up a part for my car, nothing structural, just a centre console. she has come out pretty well considering there was no vaccume on it. how ever i do have a couple of dry spots on corners and slight pin holeing on some areas. what can i do too improve the appearence of this? is it posible to wet with resin and cover with flash tape, then polish/sand back?
any ideas welcome!!!