LOL thanks for the info Tongue
 hmmm i ll go back to thinking and researching  again hahahaha


CarbonFiberCreations



neilb
neilb
Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)
Group: Forum Members
Posts: 107, Visits: 504
2 or 3 piece mould would be the best way, i wouldn't bother trying to join CF and steel together to make a wing, that means every time you want to make any you have to buy some steel ones first! defeats the point.

i can tell you that that getting a multi piece mould to seal for infusion is fun!
brasco
brasco
Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)
Group: Forum Members
Posts: 192, Visits: 305
ideas on making front fenders(you guys call them wings i think).
i dont think they can be done in one piece because of the complicated shapes. i thought of using the steel part where the part bolts to the car
and use CF for the skin where it meets the hood/bonnet and on down. --advantage to this is the part would be adjustable. in pure CF it is too stiff
to adjust like a steel part.
disadvantage-- you have to destroy a steel part to get the section with the bolt holes on it.
what about cf and a 2 part mold and bonding it together?
i dont mind going nuts for super quality, just trying to arm myself with ideas that work instead of a lot of trial and error to learn it all.

thanks everyone !


CarbonFiberCreations



GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search