Hi,
Soon I will be bonding the CF roof panel I made. It's an exact copy of the original metal panel.
The original panel was spot welded all the way around and some sort of very tough thick adhesive was used on the inside (shown in the pics) I cut this off when the roof panel was removed. 
I think I will use VM100 to bond the outer edge of the panel where it was spot welded, but I'm not sure what to use on the inside.
Any suggestions?
Attachments
16876155557890.jpg (487 views, 143.00 KB)
16876155558661.jpg (375 views, 135.00 KB)
16876155559082.jpg (367 views, 153.00 KB)
16876155559593.jpg (434 views, 132.00 KB)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search