+x Hanaldo - 1/27/2023 10:05:22 PMI'd say the majority of your problem is the bridging. When you've got major bridging like that, it will cause issues not only in that specific area, but also in the rest of the laminate as it causes uneven resin distribution within the laminate.Be 100% sure you have no bridging on your next test.