Thanks for the possitive comment,
Next thing to work on will be the "eeeuhm" inbetween the sentences BigGrin
Quit hard to improvise and think of words in an other language at the same time :p

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




brasco
brasco
Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)Supreme Being (1.4K reputation)
Group: Forum Members
Posts: 192, Visits: 305
BigGrin poor english? you are doing better than many native speakers we have here !!
and no worries !!



CarbonFiberCreations



Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
heh indeed I learn everyday a bit more about adobe aftereffects :p
last thing is the greenscreen I used for the intro...

Well indeed shrinkage tape would be great, thats why I told in the begininning I will do it on to different ways... 
but the shrinkage tape I'll do on a broken Carbon Hockey stick... to have a bit more variation Smile

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




ajb100
ajb100
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
Brilliant job!

Could you not have used high shrink tape to compress it all instead of vac bagging?
Jack.Strong
Jack.Strong
Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)Supreme Being (356 reputation)
Group: Forum Members
Posts: 52, Visits: 549
Your getting better with adobe editing Tongue
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
Hi everyone,

I've just finished a new tutorial and thought it might be worth sharing with all of you,
It's the repair of a broken Carbon Fiber Bike Frame, explained step by step.
Let me know what you think of it, did I made some mistakes?....
I know I went a little to far on the sanding, getting through the finishing layer of carbon, but shouldn't cause 
massive structural problems I think? 

Sorry for the poor english at some times and errors, but english isn't my native language and I did my best to make it understandable Smile

There is also a little publicity for Easycomposites on the pump and so on, will add the easycomposites link in the discription of the video if ok 
for easycomposites guys? Smile



Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search