Conversion Roof Targa Top To hard Top - Supra mk4
Conversion Roof Targa Top To hard Top - Supra mk4
Post Reply
Like
5
Conversion Roof Targa Top To hard Top - Supra mk4
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Dezer
Dezer
posted 4 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 74,
Visits: 1.8K
How to fill these gaps between the body and the roof without cracking over time?
(Areas circled in the image below.)
And what is the best option to glue the roof to the body and that has a good structural union?
This image is merely illustrative, but we are making a well-structured ceiling with structural cores and carbon fiber.
Reply
Like
5
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Conversion Roof Targa Top To hard Top - Supra mk4
Dezer
-
4 Years Ago
I would use a methyl-methacrylate for the structural bond. For filling the gap, you need something with good flex to avoid cracking, so a polyurethane adhesive like Sikaflex wouldn't be a terrible.....
Hanaldo
-
4 Years Ago
Methyl methacrylate was number 1 on my list of options for making the structural connection. To fill in the gaps, we would like something that could do preparation and paint on the filling, so as not...
Dezer
-
4 Years Ago
Anything rigid enough to sand and paint is very likely going to crack over time. You can paint over flexible polyurethanes, but they are much more difficult to prepare in a way that will be invisible...
Hanaldo
-
4 Years Ago
If the roof is gutted underneath, you may be able to add layers of carbon tape over the join line to stiffen the join line up even further which would reduce the chance of cracking. if its metal,...
Warren (Staff)
-
4 Years Ago
Post Reply
Like
5
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search