Group: Forum Members
Posts: 42,
Visits: 1.4K
|
Thanks for Your reply Warren. For my purpose I use your method from tutorial with house vacuum cleaner and packing bags so vacuum didn't exceeded 20% for sure.
I checked one spare section I cut from a model and it seems that it might be good actually although not 100% sure. To me it seems that if layup stayed dry, first layer is semi dry one and thats what bothers me because I am not sure how is that possible, especially with a lot of resin and vacuum. Anyhow I will try and use model, if it fails will inspecr further
|