2k clear in mould before infusing


Author
Message
carbon man
carbon man
Supreme Being (758 reputation)Supreme Being (758 reputation)Supreme Being (758 reputation)Supreme Being (758 reputation)Supreme Being (758 reputation)Supreme Being (758 reputation)Supreme Being (758 reputation)Supreme Being (758 reputation)Supreme Being (758 reputation)
Group: Awaiting Activation
Posts: 86, Visits: 1.2K
Is it possible to spray 2k clear into uni mould surface wait to dry and then use epoxy infusion resin?


Replies
Fasta
Fasta
Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
When I mould parts with Duratec as an in mould coating I still also spray a clear polyurethane on the finished parts too.




Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Fasta - 7/6/2021 9:19:37 AM
When I mould parts with Duratec as an in mould coating I still also spray a clear polyurethane on the finished parts too.



Yeh agreed, this is the best way. The Duratec gives a nice non-porous surface to sand and apply the polyurethane to, and the polyurethane provides the UV protection.

Unfortunately it is also the most costly and labour intensive, as well as the heaviest option.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
carbon man - 4 Years Ago
Fasta - 4 Years Ago
carbon man - 4 Years Ago
Hanaldo - 4 Years Ago
carbon man - 4 Years Ago
Hanaldo - 4 Years Ago
carbon man - 4 Years Ago
Fasta - 4 Years Ago
Hanaldo - 4 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search