Split mould - Infusion


Author
Message
Dezer
Dezer
Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)
Group: Forum Members
Posts: 74, Visits: 1.8K
I have a split mold that we use screws to glue the two parts (doors). However, it was pierced in an area of the flange that is hindering us to make new infusions.

Does anyone have any tips on how to temporarily close these holes and not give air leaks when closing the vacuum bag?