Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
Temporary closure could be with gum tape or bag film and gum tape over the hole. As long as the cover is leak tight you should be ok. Alternatively envelope the bag and it is not so much an issue and can be blocked with filleting wax to stop resin coming through.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|