Azzaw46 - 9/19/2021 10:33:49 PM
jamie johnson-marshall - 4/29/2021 10:28:27 AM


Sorry I don't know why the picture is the wrong way up.
You'll have issues with dry spots where the resin struggles to penetrate through tight Uni.
Even with heat and infusion resin. 

I find making Glass fins much more productive and durable. 


Jamie im a able to talk futher with you about this subject, im still playing around with it 😅

I cant actually find you on Facebook. What is the exact spelling? Carbonworkx? 
There are a few "carbon works" 

Dentex
D
Supreme Being (578 reputation)Supreme Being (578 reputation)Supreme Being (578 reputation)Supreme Being (578 reputation)Supreme Being (578 reputation)Supreme Being (578 reputation)Supreme Being (578 reputation)Supreme Being (578 reputation)Supreme Being (578 reputation)
Group: Forum Members
Posts: 42, Visits: 1.4K
jamie johnson-marshall - 9/20/2021 5:23:31 PM

I cant actually find you on Facebook. What is the exact spelling? Carbonworkx? 
There are a few "carbon works" 

I am considering somethin similiar so we can talk. I can send you my private fb profile in private message. 

Azzaw, that is not really bending as commercial flippers bend. At least couple of them that I tried, looks it could be stiff in water.