Hey guys.   Im relatively new to moulding and such.

Now i have a problem.. not sure how exactly to solve


I have a 2 part mould..   made from the easy conposites unimould system..   (all went well up to my last layup.)

Heres whats going on.   Ive made a mould that will be joined after i have layd up both halfs.(rc boat)

Ive made 3 products using hand layup without isseus and had a perfect seemline in all 3 using hand layup...

Now i made 1 vacuum infused.  And my seem was off. On both sides...  the bottom half is 0.4 to 0.5mm wider on each side then the top half..   first i didnt notice.    Trimmed it. Joined it split it and oh sh....   yes.   I thought at first that i had a pre release but apperently not.   I checked the mould.  And yes. Its deformed..(not much)...    is it possible to fix. Or do i need to make a new mould?

(I need 1 more product from it to have a plug to make a new mould. But it would be nice if i had a perfect product..
The plug i used is back to the owner.. and the perfectly straight products are sold... )
Edited 5 Years Ago by jeffrey bres
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search