Large Tube - Closed split mould


Author
Message
Robert72
R
Supreme Being (521 reputation)Supreme Being (521 reputation)Supreme Being (521 reputation)Supreme Being (521 reputation)Supreme Being (521 reputation)Supreme Being (521 reputation)Supreme Being (521 reputation)Supreme Being (521 reputation)Supreme Being (521 reputation)
Group: Forum Members
Posts: 57, Visits: 151
Well, here it is, after allowing the part to stabilise for a couple of weeks the lid is finally off. The surface finish is quite good for a newbie i think. You can see that optimum compaction has net been achieved, especially in that final picture. For several reasons however, the tube will be getting skinned with a single layer of carbon. Here's the pics:






Chris Rogers
C
Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)Supreme Being (1.2K reputation)
Group: Forum Members
Posts: 120, Visits: 933
That's beautiful!  The distortion happens - was this near the feed line?  




Robert72
R
Supreme Being (521 reputation)Supreme Being (521 reputation)Supreme Being (521 reputation)Supreme Being (521 reputation)Supreme Being (521 reputation)Supreme Being (521 reputation)Supreme Being (521 reputation)Supreme Being (521 reputation)Supreme Being (521 reputation)
Group: Forum Members
Posts: 57, Visits: 151
Chris Rogers - 3/26/2021 2:13:17 PM
That's beautiful!  The distortion happens - was this near the feed line?  

Chris, i'm not sure what end that was. Some of the cloth did not lay flat perhaps due to a combination of the thick layup and also the difficulty of managing the layup in the enclosed mould.