Hi there,
Thank you for let me join in this forum.
I'm from Italy, where we work with carbon fibers, vacuum bags etc etc, actually we made windsurfing boards and some other fiber parts.
3 months ago we upgrade the Vacuum Pump DVP LB25 ( 25m3/h) and was working fine until yesterday, that without any reason the pump start to make noise and few moment later stops working.. ( All the power went out like there was a short circuit).
We immediately unplug the pump, and power again the lights... but the pump never turn on again.
Few consideration:
Oil level okay
No Dust on the circuit
No  bad  smell
We contact immediately the dealer, but  he told us to ship over so they can check.
Meantime we need to get a back up (FAST SHIPPING AND DELIVERY) , to continue to finish some works. Seems so hard to find any "Serious Pump" on line, except on Easy Composites website, but now with BREXIT all get more expensive.
We don't need 25m3/h that allows us to vacuum 4 boards at time, but something smaller.
Do you guy can suggest us, any website where we are allowed to buy a pump, with fast shipping. although slightly less powerful compare our.
Thank you again.. for any reply.




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search