Hello everyone, my question is related to thickness availability of aluminum honeycomb core. I searched on internet and I found thickness range in between 0.25 inch to 4 inch. so what will be the increment between this range? If I want 0.4 inch thick honeycomb core or 0.5 inch thick will it be available?

Thanks.
Warren (Staff)
Warren (Staff)
Supreme Being (36K reputation)Supreme Being (36K reputation)Supreme Being (36K reputation)Supreme Being (36K reputation)Supreme Being (36K reputation)Supreme Being (36K reputation)Supreme Being (36K reputation)Supreme Being (36K reputation)Supreme Being (36K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Unfortunately we only have the metric thickness' available as you see on our website.  Currently we are not able to get any other thickness. 

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant