By Tim Ane - 1/15/2021 6:40:19 AM
Hello everyone, my question is related to thickness availability of aluminum honeycomb core. I searched on internet and I found thickness range in between 0.25 inch to 4 inch. so what will be the increment between this range? If I want 0.4 inch thick honeycomb core or 0.5 inch thick will it be available?
Thanks.
|
By Warren (Staff) - 1/20/2021 9:35:39 AM
Unfortunately we only have the metric thickness' available as you see on our website. Currently we are not able to get any other thickness.
|
|