Hi everybody,

Just asking for some help.

I want to copy the plastic ring (just the upper part). Mould worked fine but I was not able to demould the carbon copy. Could be a release agent issue but I am wondering if the form of the part makes it necessary to do a split mould...

So perhaps somebody already made parts like that and can help. And sorry, could not turn the images...


Thanks in advance and a happy new year!