Massimiliano
M
Massimiliano
posted 6 Years Ago
ANSWER
HOT
Topic Details
M
Group: Forum Members
Posts: 167,
Visits: 1.1K
Hi, my gelcoat is almost over and Easycomposites is not shipping until jan.
Is it possible to make a do-it-yourself gelcoat?
How?
Thanks
Reply
Like
9
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
DIY gelcoat
mporta71
-
6 Years Ago
Anyone?
mporta71
-
6 Years Ago
It is possible, but you need the right blend of additives. You can make do with just cab-o-sil (fumed silica), but it doesn't really make a gelcoat.
Hanaldo
-
6 Years Ago
Do you have a list of such additives? Epoxy tooling gelcoat, besides the fact the I am out of stock at the moment, is really expensive and sometimes I need something for a one off mould that will be....
mporta71
-
5 Years Ago
Fumed silica is virtually essential to make a thixotropic paste. Calcium carbonate will increase the hardness and gloss retention. Graphite powder will give you a nice slick dark grey/black surface.....
Hanaldo
-
5 Years Ago
Thanks, very kind as usual. I agree,.this is sort of "emergency" because in this Xmas time most warehouse are closed. I had on order the gelcoat from Ec but brexit stepped in.
mporta71
-
5 Years Ago
Post Reply
Like
9
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search