Hello everybody I'm an italian luthier specialized in ukulele making, and I've been experimenting with composites for about a year. I'm now building jute+epoxy ukuleles using resin infusion but, even if I thought I found a consistent method to make them, I realized it was just beginner's luck and there are a LOT OF THINGS I still don't understand about infusion.
So..here I am looking for some advices!
I'll start a topic explaining all my problems (infusion related ones Smile )
Here you can see the jute/epoxy ukuleles I'm making.

Ciao!






Hanaldo
Hanaldo
Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)Supreme Being (24K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Gorgeous, I love em.
Rosta Spicl
Rosta Spicl
Supreme Being (600 reputation)Supreme Being (600 reputation)Supreme Being (600 reputation)Supreme Being (600 reputation)Supreme Being (600 reputation)Supreme Being (600 reputation)Supreme Being (600 reputation)Supreme Being (600 reputation)Supreme Being (600 reputation)
Group: Forum Members
Posts: 54, Visits: 250
Pretty cool...
I'm just working on carbon fibre acoustics guitar, steel string, absolutely no wood. But autoclave technology based on carbon fibre prepregs.


Marco Todeschini
M
Supreme Being (102 reputation)Supreme Being (102 reputation)Supreme Being (102 reputation)Supreme Being (102 reputation)Supreme Being (102 reputation)Supreme Being (102 reputation)Supreme Being (102 reputation)Supreme Being (102 reputation)Supreme Being (102 reputation)
Group: Forum Members
Posts: 7, Visits: 328
Very cool guitar shape! Unfortunately I'm still too traditionalist to completely leave my beloved wood Smile 