By Marco.T - 12/10/2020 8:01:12 PM				
            
                      
            Hello everybody I'm an italian luthier specialized in ukulele making, and I've been experimenting with composites for about a year. I'm now building jute+epoxy ukuleles using resin infusion but, even if I thought I found a consistent method to make them, I realized it was just beginner's luck and there are a LOT OF THINGS I still don't understand about infusion. So..here I am looking for some advices! I'll start a topic explaining all my problems (infusion related ones   ) Here you can see the jute/epoxy ukuleles I'm making.
  Ciao!
 
  
  
  
  
  
           
		 | 			
		 
	
		
				      		    
		
		
            
            
            By Marco.T - 12/11/2020 3:31:08 PM				
            
                      
            Very cool guitar shape! Unfortunately I'm still too traditionalist to completely leave my beloved wood   
           
		 | 			
		 
	
	
						
		 	
		
	 |