Plaster of paris? No. It is highly porous, so it would need to be sealed. You could maybe use plaster of paris and then wrap it in Teflon tape/glass, but it wouldn't leave a nice surface finish. Possibly an option for non-aesthetic parts, but not a great one. It doesn't have a fantastic CTE either, so probably a few issues there.
|