megagrumpy
megagrumpy
posted 14 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 1,
Visits: 8
I need to make a cowl for an RC aircraft that is relatively small and light. On one site they advise 6 oz or even 4 oz Glass fibre cloth. What would be a suitable carbon cloth for this job?
Reply
Like
9
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Best cloth for small cowl for RC aircraft
megagrumpy
-
14 Years Ago
Hi, 6oz is 170g, 4oz is 113g. If you did want to use glass then we have a 100g Woven Glass Fabric...
Matt (Staff)
-
14 Years Ago
Post Reply
Like
9
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search