shkolyar
s
shkolyar
posted 6 Years Ago
ANSWER
HOT
Topic Details
s
Group: Forum Members
Posts: 1,
Visits: 46
I would like to ask you,
1. How did they make such clips?
2. Сan it be done only with pre-preg? or somehow with resin infusion?
Reply
Like
7
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Front bumper grille frame
shkolyar
-
6 Years Ago
Not the best picture but from zooming in they look like carbon. So either cut out from flat sheet and bonded into place or what looks more likely, they were moulded that way around the mould...
Warren (Staff)
-
6 Years Ago
Hi Looking the picture and I may be wrong, the distortion on the inside fabric reflections and levels, these clips are prefab and inserted into mold. I guess they manufactured the outside skin by...
torstenker
-
6 Years Ago
+ x [quote] [b] torsten Ker - 10/13/2020 10:30:31 PM [/b] Hi Looking the picture and I...
torstenker
-
6 Years Ago
Post Reply
Like
7
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search