Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Mould Making
»
Advanced silicone mould
Advanced silicone mould
Post Reply
Like
7
Advanced silicone mould
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
arntr
arntr
posted 6 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 4,
Visits: 21
Hi.
Is it possible to get some tips making an advanced silcone mould. I am trying to make Mud flaps wich is no longer produced. The idea is to use polyurethane to make the flaps.
The mould must take care of both the outer shape and the inner shape of the part. Have a look at the attached pictures. Which one of the polyurethane castin resins is best suited?
Thanks!
Reply
Like
7
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Advanced silicone mould
arntr
-
6 Years Ago
I would consider a split mould that is silicone faced and supported by fibreglass backing mould too. It's quite an involved and long process with flanging, silicone brushing and fibreglass, then...
Fasta
-
6 Years Ago
Thanks for answer. Just to make sure I understand this right. Making a split mould with silicon face. Put the two (inner and outher) together and fill the hole thing withpolyurethane? Any suggestion....
arntr
-
6 Years Ago
That's right, I only say to use silicone since the back side of your part may have lots of details and these can possibly be cast ok as you will be able to flex the silicone off the new cast part? If...
Fasta
-
6 Years Ago
Post Reply
Like
7
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search