Group: Forum Members
Posts: 59,
Visits: 278
|
2 years ago I did a fighter jet model fuselage in plaster as a template. I thinly painted the dried plaster with wood hardener (similar to the S120 Advanced Board & Mould Sealer), then spayed it with 2k epoxy primer, sanded with 1200 wet paper and used release wax and PVA The resulting mould came off the template without big issues
|