Hi everyone,
 
Thanks for having me. I have recently started playing with carbon fiber and am here to share what little knowledge and experience I have. More importantly, I am also here to learn from my mistakes and others who are more experienced.

My current project is a rear diffuser that I did skinned in carbon fiber. It was my first attempt and those YouTube videos make it look easy. I definitely learned a lot and I really enjoyed it. The part didn't come out the best but it was extremely complex for first project. 


thanks again for having me. 
taimur
t
Supreme Being (488 reputation)Supreme Being (488 reputation)Supreme Being (488 reputation)Supreme Being (488 reputation)Supreme Being (488 reputation)Supreme Being (488 reputation)Supreme Being (488 reputation)Supreme Being (488 reputation)Supreme Being (488 reputation)
Group: Forum Members
Posts: 32, Visits: 122
Mo_Carbon - 9/7/2020 9:27:34 AM
Hi everyone,
 
Thanks for having me. I have recently started playing with carbon fiber and am here to share what little knowledge and experience I have. More importantly, I am also here to learn from my mistakes and others who are more experienced.

My current project is a rear diffuser that I did skinned in carbon fiber. It was my first attempt and those YouTube videos make it look easy. I definitely learned a lot and I really enjoyed it. The part didn't come out the best but it was extremely complex for first project. 


thanks again for having me. 


Thanks for sharing here. Waiting for your video!

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search