Kacordy - 9/4/2020 5:51:22 PM
I just bought this complete vacuum bagging system. It’s brand new. I cannot get the gauge on the pot that catches the excess resin to show the negative vacuum pressure? The pump works and pulls and holds vacuum in the pot. I can release the clamp I have on the hose that goes to the bag and it relieves the pot of vacuum when released. What am I doing wrong? Thanks, Allen

Ok, I finally figured it out. I had the lines crossed. 

Kacordy
K
Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)Supreme Being (273 reputation)
Group: Forum Members
Posts: 17, Visits: 341
I just bought this complete vacuum bagging system. It’s brand new. I cannot get the gauge on the pot that catches the excess resin to show the negative vacuum pressure? The pump works and pulls and holds vacuum in the pot. I can release the clamp I have on the hose that goes to the bag and it relieves the pot of vacuum when released. What am I doing wrong? Thanks, Allen